Download Solution PDFThe soldering process is carried out in the temperature range
Answer (Detailed Solution Below)
Detailed Solution
Download Solution PDFExplanation:
The soldering process is carried out generally in the temperature range of 180 – 250° C which is sufficient to melt the solder material. Most solders are alloys of lead and tin. Three commonly used alloys contain 60, 50, and 40% tin and all melt below 240°C.
In soldering, Solder Flux is used. Most commonly used soldering flux is as followed
- Ammonium chloride or rosin for soldering tin
- Hydrochloric acid and zinc chloride for soldering galvanized iron
Last updated on Jun 2, 2025
-> The RRB NTPC Admit Card 2025 has been released on 1st June 2025 on the official website.
-> Railway Recruitment Board activated the RRB ALP application form 2025 correction link, candidates can make the correction in the application form till 31st May 2025.
-> The Railway Recruitment Board (RRB) has released the official RRB ALP Notification 2025 to fill 9,970 Assistant Loco Pilot posts.
-> The Railway Recruitment Board (RRB) has released the official RRB ALP Notification 2025 to fill 9,970 Assistant Loco Pilot posts.
-> The official RRB ALP Recruitment 2025 provides an overview of the vacancy, exam date, selection process, eligibility criteria and many more.
->The candidates must have passed 10th with ITI or Diploma to be eligible for this post.
->The RRB Assistant Loco Pilot selection process comprises CBT I, CBT II, Computer Based Aptitude Test (CBAT), Document Verification, and Medical Examination.
-> This year, lakhs of aspiring candidates will take part in the recruitment process for this opportunity in Indian Railways.
-> Serious aspirants should prepare for the exam with RRB ALP Previous Year Papers.
-> Attempt RRB ALP GK & Reasoning Free Mock Tests and RRB ALP Current Affairs Free Mock Tests here